Glastar Pressure Pot replacement parts

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Phil Hoppes
Posts: 298
Joined: Wed Mar 12, 2003 2:20 pm
Location: Overgaard, AZ

Glastar Pressure Pot replacement parts

Post by Phil Hoppes »

So I'm guessing it has been at least 10 maybe even 15 years since I've posted on this board. LOL. So I'm firing up my studio again and my old Glastar sandblaster is in need of replacement parts. I see via "The Google" that they have gone out of business. I've been searching but I'm not finding any company that either bought them or is making replacement parts for their equipment. Looks like this board has really quite gone down in activity since then. Perhaps someone will see and respond. Alas, Tony Smith, the resident sandblasting expert has passed on. I miss Tony every day. He was an inspiration to us all.
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Glastar Pressure Pot replacement parts

Post by Kevin Midgley »

this site may have the answers.
TheSandWitch.com
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Glastar Pressure Pot replacement parts

Post by Brad Walker »

Phil,

The Glastar sandblaster used to be made by TPTools. Perhaps they can help with parts.

https://www.tptools.com/
Post Reply