Is there anything I need to check before I test my kiln ( Glass Glow) after not using it for 10 years? It's got a nice Paragon controller that I don't want to mess up!
Kiln Question
Moderators: Brad Walker, Tony Smith
-
Mark Hughes
- Posts: 49
- Joined: Mon Mar 17, 2003 6:27 pm
- Location: Omaha, Nebraska
Kiln Question
I am finally getting back to fusing after a long break.
Is there anything I need to check before I test my kiln ( Glass Glow) after not using it for 10 years? It's got a nice Paragon controller that I don't want to mess up!
Is there anything I need to check before I test my kiln ( Glass Glow) after not using it for 10 years? It's got a nice Paragon controller that I don't want to mess up!
Mark Hughes
Re: Kiln Question
I have no suggestions. But welcome back!
-
Brad Walker
- Site Admin
- Posts: 1543
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Kiln Question
Put some scrap glass in it. Small pieces, two layers thick, in various places in the kiln. Fire to a full fuse and see what happens. It will tell you if the kiln is working fine and if it heats uneven.Mark Hughes wrote: ↑Sat Aug 19, 2023 12:57 pm I am finally getting back to fusing after a long break.
Is there anything I need to check before I test my kiln ( Glass Glow) after not using it for 10 years? It's got a nice Paragon controller that I don't want to mess up!![]()
-
Mark Hughes
- Posts: 49
- Joined: Mon Mar 17, 2003 6:27 pm
- Location: Omaha, Nebraska