Tack fusing holey moley molds: Any reasons not to?
Posted: Tue Dec 12, 2023 6:04 pm
				
				I’ve been using holey moley frit molds lately while eyeing some colorful batches of minis gathered from nipping that I’ve  been wanting to play with.  I was curious about what would happen in a high tack fuse, so they looked like a bunch of tiny gems. i’m not finding any comments  about it or photos  online.  Thoughts?
I’m imagining that it could be a lumpy mess if filled up to the usual amount, mushed on the bottom and more relief on the top. Unless it’s very lightly, tacked, in which case it would probably be sharp —?
if i just covered the bottom of the pod so not too thick, might that yield something interesting?
Ideas for firing schedules?
If you experimented with this or know of any references online, I'd be interested to see.
			I’m imagining that it could be a lumpy mess if filled up to the usual amount, mushed on the bottom and more relief on the top. Unless it’s very lightly, tacked, in which case it would probably be sharp —?
if i just covered the bottom of the pod so not too thick, might that yield something interesting?
Ideas for firing schedules?
If you experimented with this or know of any references online, I'd be interested to see.