Can I refire?

Posted: Thu Feb 26, 2004 1:56 pm
by Jan Daniel
I am brand new to slumping bottles and love it. Can anyone help me.....one of the bottles...a grey goose...did not flatten enough at the bottom. Can they be refired? At the same temp.? Thank you so much. :) [/quote]

Posted: Thu Feb 26, 2004 2:05 pm
by dan
fire away ,maybe knock up the temp a wee bit or soak a bit longer.you could always have a peek in at top temp and see if its flattening as much as you'd like

Posted: Thu Feb 26, 2004 2:07 pm
by charlie
you may have to slow down a bit. note that your bottle now may have a thicker place than it was, and thick glass takes longer to get up to temp. going too fast may thermal shock it.

Posted: Mon Mar 08, 2004 1:11 am
by Jan Daniel
charlie wrote:you may have to slow down a bit. note that your bottle now may have a thicker place than it was, and thick glass takes longer to get up to temp. going too fast may thermal shock it.
Charlie, Thank you so much for your help. I appreciate it and will fire away. Again, many thanks. Jan

Posted: Mon Mar 08, 2004 1:11 am
by Jan Daniel
dan wrote:fire away ,maybe knock up the temp a wee bit or soak a bit longer.you could always have a peek in at top temp and see if its flattening as much as you'd like
Dan,
Thanks much for your help. Appreciate it and will refire. Thanks again,
Jan