kiln wash and clay mold

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
dplastre
Posts: 1
Joined: Sat Sep 14, 2024 4:03 pm

kiln wash and clay mold

Post by dplastre »

do i need kilnwash with clay mold when firing float glass
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: kiln wash and clay mold

Post by Brad Walker »

Yes.
Post Reply