What to use on a 3mm piece of base and 3mm dichro

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Karen Avery
Posts: 3
Joined: Fri Nov 01, 2024 2:55 pm

What to use on a 3mm piece of base and 3mm dichro

Post by Karen Avery »

I am going to make a plate with a base piece of 3mm black glass and a layer of 3mm dichro down the middle. I was planning on putting a 3mm piece of clear class over it all but am afraid of the space that is between the top and bottom pieces (the base and the cap). What can I put on the black glass before firing so that it doesn't make a lot of bubbles? I am going to slump it after so need to do a full fuse. It is System 96.
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: What to use on a 3mm piece of base and 3mm dichro

Post by Brad Walker »

Put the clear below the black, not on top.
Karen Avery
Posts: 3
Joined: Fri Nov 01, 2024 2:55 pm

Re: What to use on a 3mm piece of base and 3mm dichro

Post by Karen Avery »

If I put it under the black, the dichro won't have any protection on it. I guess I will have to do that though.
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: What to use on a 3mm piece of base and 3mm dichro

Post by Brad Walker »

You can sift a very thin layer of clear powder (two grains thick at most) over the entire top of the piece.

Or use dichro on clear and fire upside down.
Post Reply