Post by Terry Gallentine »

I have a need for a tape that I can temporarily tape glass pieces together before fusing. I have seen in older posts, the use of Scotch tape but I was wondering what the current information is regarding this. Is there something new that is better than Scotch tape?
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Clean Burning Tape

Post by Brad Walker »

We've had good luck with both scotch tape and clear packing tape. Just don't lay it on too thick.
Terry Gallentine
Posts: 195
Joined: Mon Jul 19, 2004 2:08 pm
Location: River Falls, WI
Contact:

Re: Clean Burning Tape

Post by Terry Gallentine »

I will give the scotch tape a try. Thanks Brad.