No Days glass fusing glue

Posted: Sun Jun 08, 2025 10:54 am
by Terry Gallentine
Does anyone have any experience with No Days glass fusing glue? I need a glue that is not water soluble like Glastac is and I have read that No Days is not water soluble. Are there other alternatives to Glastac that are not water soluble and not the older suggestions such as super glue?

Re: No Days glass fusing glue

Posted: Wed Jun 11, 2025 2:58 pm
by Brad Walker
You might ask the No Days people: https://nodaysadhesives.com/No-Days-Liq ... g-c5749935

Don't know if it will work for you, but hot glue is polymer based so shouldn't be water soluble. It burns off pretty clean, but you may want to test for your application if you try it.

Re: No Days glass fusing glue

Posted: Wed Jun 11, 2025 5:25 pm
by Terry Gallentine
Thanks Brad.

Re: No Days glass fusing glue

Posted: Tue Jun 24, 2025 11:46 am
by Vonon
I've used hot glue without a problem.