Heating Elements

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Renee S
Posts: 3
Joined: Tue Mar 11, 2003 10:02 am
Location: Illinois

Heating Elements

Post by Renee S »

Fired my kiln for the first time last night. I was drying my shelf so I only had to fire to 500 degrees for about 30 min. While looking in the kiln I notifce that only the top elements were on. My question is are all the elements supposed to fire at the same time or do they fire at different times depending on what temp. you are firing to :?: My kiln is a Jen-Ken 18" dia. (RTC-18-E) with a 12 Key Bartlett Digital Controller (RTC-1000)
Thanks Renee :wink:
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

elementary, Watson

Post by Marty »

Check the manual? Call the dealer? Call Jen-Ken?

I would expect all the elements to go on together. An override for something like drop ring slumps would be nice too.
Post Reply