A-14
Anybody been using Thompsons A-14? I was using it today with the screening and painting paint and it seems like it's taking forever to dry. Probably because I have to slump this tray and be done by tomorrow. Any harm in firing it a bit wet?
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
Re: A-14
Yes, it may be slow drying but it beats having to clean the screen after each piece.Becca wrote:Anybody been using Thompsons A-14? I was using it today with the screening and painting paint and it seems like it's taking forever to dry. Probably because I have to slump this tray and be done by tomorrow. Any harm in firing it a bit wet?
It takes about 3-4 hours to dry by itself. Heat in the kiln to speed it up. Maybe 150-175 f for 15 min.
Ron
-