Looking for small molds for firing

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
candala
Posts: 28
Joined: Tue Mar 25, 2003 7:44 am

Looking for small molds for firing

Post by candala »

Hi, I have a 7 inch shelf, small kiln. Where can I find (other than Ebay) small molds of rectangles, hearts, etc. for me to put scrap in and fire in the kiln? Thanks.
Colin & Helen

Post by Colin & Helen »

Why not cut the shape out of fibre board.

Colin
candala
Posts: 28
Joined: Tue Mar 25, 2003 7:44 am

Post by candala »

Out of fiberboard? I want the depth as well, similar to a stainless steel mold. Thanks anyway.
Jackie Beckman
Posts: 475
Joined: Sun Mar 09, 2003 5:01 pm
Location: Arizona
Contact:

Post by Jackie Beckman »

Gil is selling some small molds at Fusion HQ - I saw them at my local distributor, and I'm sure you can get them on his site. He's a sponsor of the board, just click on his link above
KatyPattison
Posts: 21
Joined: Sun Mar 09, 2003 4:51 pm
Location: Canada
Contact:

Post by KatyPattison »

I have made small molds (for lamp repairs) out of clay. Roll it flat (I use spacers on the counter to get a uniform thickness), shape it over a shape you like that is covered with saran wrap and cover lightly so it can dry slowly. You can sand it at this point to smooth it out if necessary. Drill your holes and then bisque fire (or take it to a pottery shop and have them bisque fire a bunch for you at one time). They don't last as long as commercially made molds but work just fine.
Katy
Fusionistic
Posts: 7
Joined: Sun Mar 30, 2003 12:30 pm

Post by Fusionistic »

Katy Pattison wrote:I have made small molds (for lamp repairs) out of clay. Roll it flat (I use spacers on the counter to get a uniform thickness), shape it over a shape you like that is covered with saran wrap and cover lightly so it can dry slowly. You can sand it at this point to smooth it out if necessary. Drill your holes and then bisque fire (or take it to a pottery shop and have them bisque fire a bunch for you at one time). They don't last as long as commercially made molds but work just fine.
Katy
Katy -- any reason you stop at bisque firing the molds? Would they not last longer if you high-fired them?

I have been thinking of creating my own molds. I was planning on using a friends pottery kiln and firing them twice (bisque and high).
Doug Bailey
Jerry

Small Molds

Post by Jerry »

Bisque firing is a generic term used to designate the process of firing clay to a temperature higher than you ever plan to go again. In pottery we bisque to about 2000 for planned glases that mature at 1875.

For a slumping mold where you probably will never go much over 1500 degrees, bisque firing could be anything over 1600. The higher the better. Higher temps will make a longer lasting mold; I've got some I've been using for at least 10 years. Make sure to use a heavy grog clay like raku clay; it doesn't crack up as much during drying and seems to have an indefinate life span.

Jerry
Valerie
Posts: 42
Joined: Sun Mar 09, 2003 7:01 pm
Location: Kentwood Michigan

molds

Post by Valerie »

alpineglass.com has lots of molds
ceramic & stainless...I buy greenware at my local ceramic shop and fire to bisque. Target , KMart all have stainless stuff you can convert to molds.
:idea:
Fusionistic
Posts: 7
Joined: Sun Mar 30, 2003 12:30 pm

Re: Small Molds

Post by Fusionistic »

Jerry wrote:Bisque firing is a generic term used to designate the process of firing clay to a temperature higher than you ever plan to go again. In pottery we bisque to about 2000 for planned glases that mature at 1875.

For a slumping mold where you probably will never go much over 1500 degrees, bisque firing could be anything over 1600. The higher the better. Higher temps will make a longer lasting mold; I've got some I've been using for at least 10 years. Make sure to use a heavy grog clay like raku clay; it doesn't crack up as much during drying and seems to have an indefinate life span.

Jerry
OK, I guess I didn't understand that. I had thought that the first firing (prior to applying glaze) was to a lower temperature than the glaze firing.
Doug Bailey
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: Small Molds

Post by rosanna gusler »

Fusionistic wrote:
Jerry wrote:Bisque firing is a generic term used to designate the process of firing clay to a temperature higher than you ever plan to go again. In pottery we bisque to about 2000 for planned glases that mature at 1875.

For a slumping mold where you probably will never go much over 1500 degrees, bisque firing could be anything over 1600. The higher the better. Higher temps will make a longer lasting mold; I've got some I've been using for at least 10 years. Make sure to use a heavy grog clay like raku clay; it doesn't crack up as much during drying and seems to have an indefinate life span.

Jerry
OK, I guess I didn't understand that. I had thought that the first firing (prior to applying glaze) was to a lower temperature than the glaze firing.
it can go either way, stoneware and porcelain clays are usually bisqued lower than the glaze/maturing fire. rosanna
Linda Reed
Posts: 54
Joined: Fri Mar 14, 2003 6:27 pm
Location: Santa Rosa, California, USA
Contact:

Post by Linda Reed »

We have a local ceramics shop that sells bisque ware that I guess people buy and paint or something, but they have TONS of small shapes that can be used as molds (hearts, ruffles, bowls, ovals, christmas ornaments, etc). I bet you can find places on the web. I buy some component stuff from Aftosa - they have a bisqu ware section too. Also haunt thrift shops (or mega stores if you are into that type of thing) for baking type/ decor metal things. Heat, kiln wash and go. Just don't use aluminum. (Am I right? No aluminum? You can tell if a magnet won't stick??)

Linda
PDXBarbara
Posts: 292
Joined: Sun Mar 09, 2003 4:09 pm
Location: Portland, OR

Post by PDXBarbara »

Magnets don't stick to stainless either.
BB
(Am I right? No aluminum? You can tell if a magnet won't stick??)

Linda[/quote]
Barbara Bader
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

PDXBarbara (Bader) wrote:Magnets don't stick to stainless either.
BB
Some stainless steel is magnetic and some is non-magnetic. The magnetic variants have chromium and sometimes carbon, the non-magnetic have more chromium and add nickel. It's the nickel that turns the material from magnetic to non-magnetic.

Many good stainless steel molds are 18/8, which means they contain 18% chromium and 8% nickel. In addition to making them non-magnetic, this alloy makes them more corrosion resistant and more ductile (easily formable into shapes).
tom suter
Posts: 55
Joined: Sun Mar 09, 2003 8:12 pm
Location: springfield il
Contact:

Small Molds

Post by tom suter »

You might want to try this link they have several small molds and there prices are not toohigh.