Actually, sometimes water will break down the glue. Try soaking the piece in as warm water as you think it can stand and keep it up until the glue releases. Use a razor blade to start the separation. Hope that helped. - Barbara
I work with UV glues all the time. They are not guaranteed to stay stable in a wet environment, and I have had them separate under wet conditions. This led me to my response. - Barbara
Thanks for the input. I'll try the alcohol. What temp do you think it would take to break the glue down in the kiln? I tried 350 F for 4 min. Now after trying to soak it in hot water, I wonder if I made it stronger. I put it in the dishwasher with the heated water option on ... still stuck. I guess I can really do a good job of glueing. My customer should be encouraged at the quality and durability. Too bad it's crooked!!!!
TrishV