Page 1 of 1
Q-using copper and maganese carbonate in glass
Posted: Wed Apr 09, 2003 7:54 pm
by dave laporta
I know there is alot in the archives on this topic but what I did not see is how I apply them. I just did a test firing with float glass (top temp being 1515) and the results were pretty lame. all but one tile turned a dark, metal like black finish... real ugly. the one that sort-of came out only started to turn the greenish blue color when it was just a sprinkle of the powder. What I did was apply it between the sheets in varing thickness to try to understand what my tolerences were. Other tiles that the layer was on the thick side did not allow the glass to fuse fully and the chemical leaked out- agh :? Overall I did not get a mix or blend of materials. Should I be? Is there an ideal temp?
In the archives I did see one mention of using a flux or mixing it with hot water then spray it on. Can anyone shed some detailed light on this? TIA- Dave
Re: Q-using copper and maganese carbonate in glass
Posted: Thu Apr 10, 2003 4:08 am
by Brian and Jenny Blanthorn
dave laporta wrote:I know there is alot in the archives on this topic but what I did not see is how I apply them. I just did a test firing with float glass (top temp being 1515) and the results were pretty lame. all but one tile turned a dark, metal like black finish... real ugly. the one that sort-of came out only started to turn the greenish blue color when it was just a sprinkle of the powder. What I did was apply it between the sheets in varing thickness to try to understand what my tolerences were. Other tiles that the layer was on the thick side did not allow the glass to fuse fully and the chemical leaked out- agh

Overall I did not get a mix or blend of materials. Should I be? Is there an ideal temp?
In the archives I did see one mention of using a flux or mixing it with hot water then spray it on. Can anyone shed some detailed light on this? TIA- Dave
I have posted a lot on this
Realy is a big subject
First what do U want 2 achive ??
Body stains / onglaze + flux will give less bubbles
U need flux 2 melt the materials in
The higher temp U go the more disolved but the more bubbles + other problems
Thry a search on
Body stains / onglaze look out 4 some of my long posts on this