				I have not been able to find the perfect way to bond a silver bail to the back of a fused glass pendant.   Can someone suggest a type of glue or epoxy that works best for them?  I have been using 2-part epoxy but I've noticed that it doesn't take too much force to separate it from the glass.  Any suggestions are greatly appreciate.  Thanks in advance!   

 
			
					
				
				Posted: Mon Apr 05, 2004 11:01 pm
				by Cher
				Don't know about perfect, but E6000 gets recommended a lot.  Trick with that is to leave it alone for 24 hours.  (sets quicker than that)  silicone is also highly recommended.  Good luck.
			 
			
					
				Re: Glass Glue
				Posted: Mon Apr 05, 2004 11:33 pm
				by Paul Tarlow
				There are many, many threads on this in the archive.
You may want to start here:
http://www.warmglass.com/phpBB/viewtopic.php?t=829
- Paul
Laura Dawson wrote:I have not been able to find the perfect way to bond a silver bail to the back of a fused glass pendant.   Can someone suggest a type of glue or epoxy that works best for them?  I have been using 2-part epoxy but I've noticed that it doesn't take too much force to separate it from the glass.  Any suggestions are greatly appreciate.  Thanks in advance!   

 
 
			
					
				
				Posted: Mon Apr 05, 2004 11:58 pm
				by Claudia Whitten
				Laura,
  I had the same problem with pendants. I found that the earrings worked just fine with the 2 part epoxys. For the pendants I have changed to Dymax 621. I have been very pleased with it. I use an activator with it 535-A. I got my glue from Dewey Associates, 1-800-448-2306. 