Cutting BE Blue Opal, Plum 2100 series..help please
Posted: Fri Apr 11, 2003 2:49 pm
I'm trying to cut the BE opal glass, 2100 series, into a circle. I used my trusty circle cutter and did the tap, tap, tap, and not results. This glass did not seem to run along the score, and did not want to break. SO my one circle ended up in 3 pieces. I don't want to ruin the whol beautiful sheet of this glass, I have other opals, how do I cut It??? Thanks 