Hello all,
I've made what might be considered a monster of a pattern bar - at least for my little kiln!
I need to find a tile saw that can cut 2 inch depth. My lapidary trim saw has a maximum of about 1" ... and the model I have looked at at Harbor Freight is 5/8 inch depth.
Anyone have recommendations for a deep cutting tile saw? I presume they are out there ... what do the MK's cut? I have been thinking of getting one of those, but I'm wrestling between sandblasting and cutting! Both are current needs/wants.
Thanks for any thoughts,
Sadie
tile saw depth
Moderators: Brad Walker, Tony Smith
-
sadiesjewels
- Posts: 48
- Joined: Mon Mar 10, 2003 2:02 pm
- Location: N. CA
- Contact:
-
Lisa Allen
- Posts: 212
- Joined: Sun Mar 09, 2003 3:23 pm
- Location: Memphis, TN
- Contact:
Hi Sadie
My MK-370 will cut up to 1 3/4ths", but I think that the MK-100 might go up to 3 or 3 1/2"?
Lisa
My MK-370 will cut up to 1 3/4ths", but I think that the MK-100 might go up to 3 or 3 1/2"?
Lisa
Lisa Allen
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Go to your local Home Depot or tool rental center and rent an MK100 which has a 10" blade. It'll go the job just fine. Depth of cut is 3 3/4 inches. http://www.mytoolstore.com/mk/100.html
Tony
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
gone
Here's another good one (the FTS-150)
http://www.masterwholesale.com/felk/fel ... _saws.html
The blade that comes with it cuts beautifully. I'm very happy with this one.
Els
http://www.masterwholesale.com/felk/fel ... _saws.html
The blade that comes with it cuts beautifully. I'm very happy with this one.
Els
Just got a Chicago Electric 10" from harbor freight and it is great on those 2" bars will cut 3 3/4" need to have a glass blade so I just ordered one from Hisglassworks. I looked on ebay and watched the Mk100 go from 99.00 to 410. and checked the internet and always ended up back to harbor freight. They had the best price for the depht I was wanting and the power also. 2.5 hp Hope this helps, now since I saved on the saw,
I can get my sandblasting equipment! 