Hello,
I am using using the cement mold mix from Boyce Lundstom's glass fusing book 1. I am getting a bowing in flat molds that are 9 ish inches and longer.
Does anyone know why this is happening and how to reduce/eliminate it?
Mold mix formula:
6 parts calcium aluminate
3 parts sand
2 parts vermiculite
1 part fire clay
Any ideas whould be appreciated.
Thanks,
Don
Cement Mold Issue
Moderators: Brad Walker, Tony Smith
-
Barbara Cashman
- Posts: 151
- Joined: Sun Mar 09, 2003 5:42 pm
- Location: Greensboro NC
- Contact: