copper oxide
Posted: Mon May 05, 2003 1:35 am
O.K. Here I go again. Getting tired of me?
Reading the archives, it suggested mixing flux with copper oxide. In what proportions? Someone also suggested using borax to brighten the color. Guess this is another proportion
Having trouble with my hands keeping up with my head.
Kay
Reading the archives, it suggested mixing flux with copper oxide. In what proportions? Someone also suggested using borax to brighten the color. Guess this is another proportion
Having trouble with my hands keeping up with my head.
Kay