What metals can I use when slumping?
Thanks
Deborah
Can I use steel pipe for slumping? What metals can I use?
Moderators: Brad Walker, Tony Smith
-
deborahbur
- Posts: 51
- Joined: Thu Apr 10, 2003 2:09 pm
- Location: Tiverton, Rhode Island
- Contact:
-
Stuart Clayman
- Posts: 224
- Joined: Mon Mar 31, 2003 12:35 pm
- Location: Virginia
- Contact:
You can also put kiln paper coating the inside of the pipe
and then fill it with glass.
-
Mike Byers
- Posts: 56
- Joined: Mon Mar 10, 2003 6:57 pm
- Location: west central Indiana
- Contact:
Stainless steel is best, but you can use other types of steel, too. Since non-stainless steel will rust when heated, you may have to remove the rust and shelf primer after each firing. I'd avoid plated steel or galvanized steel, as you can get toxic outgassing from the plating. Even stove pipe (supported and reinforced so it won't sag when heated) is useful for forming larger-radius curves.