table top draping Q

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

table top draping Q

Post by rosanna gusler »

hi all, i am designing some small table tops. i want to do a drape type thing with the edge. say an inch and a half or so drape all the way around. so what do you think would be a good material to make my mold with? mild steel? rigidised fiber? plaster? anybody got a learning curve to share? thanks, rosanna
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: table top draping Q

Post by Bert Weiss »

rosanna gusler wrote:hi all, i am designing some small table tops. i want to do a drape type thing with the edge. say an inch and a half or so drape all the way around. so what do you think would be a good material to make my mold with? mild steel? rigidised fiber? plaster? anybody got a learning curve to share? thanks, rosanna
Rosanna

I would use Unifrax HD board. I sometimes cover it with fiberfrax blanket coated with alumina powder. You didn't mention what kind of glass. If it is float, and you are not fusing I would fire to 1365 and soak until you like the look. If you are fusing float, fire to 1420.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: table top draping Q

Post by Brad Walker »

rosanna gusler wrote:hi all, i am designing some small table tops. i want to do a drape type thing with the edge. say an inch and a half or so drape all the way around. so what do you think would be a good material to make my mold with? mild steel? rigidised fiber? plaster? anybody got a learning curve to share? thanks, rosanna
Read this: http://www.kerseyglass.com/resource-cen ... ticle2.asp
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Post by rosanna gusler »

ok, thanks. i will try the steel first since i live in the land of metal shops. time to go hit the ole scrap piles. rosanna
Post Reply