Bullseye starts moving for casting above 920 c (1700 f), at 980 c (1800 f) it flows nicely.Colin wrote:Helen wants me to cast a couple pieces ....in non Pb glass.. so our glass choice is Bullseye ..crushed up sheets and scrap... my question is what is the flow temperature. for BE ( I haven't used BE for some time and have also lost all my records from previous firings for this glass)..Colin
Hi ColinColin wrote:Thanks Ron.. I will keep you posted re the results..Colin..
![]()