A-14?
Moderator: Tony Smith
-
Nancy Juhasz
- Posts: 113
- Joined: Sun Mar 09, 2003 10:10 pm
- Location: Ohio
A-14?
I’m returning to fused glass from a long absence. I found something called A-14. What is it? No instructions on bottle.
Re: A-14?
A13 Is an acrylic medium from Thompson Enamel. There. Thats infinitely helpful, isn't it?
Re: A-14?
I thought it was a Bingo number....Don Burt wrote:A13 Is an acrylic medium from Thompson Enamel. There. Thats infinitely helpful, isn't it?
Re: A-14?
BangoAndyT wrote:I thought it was a Bingo number....Don Burt wrote:A13 Is an acrylic medium from Thompson Enamel. There. Thats infinitely helpful, isn't it?
-
Nancy Juhasz
- Posts: 113
- Joined: Sun Mar 09, 2003 10:10 pm
- Location: Ohio
Re: A-14?
Thanks , I guess! Your right no help. I bought this stuff maybe 10-20 years ago from Brad and don’t see it any more and can’t for the life of me remember what it is/was for
Re: A-14?
It's for sale here on Warmglass.com. Still don't know what it is. I know it's not for Bingo. Down at the bottom of the enamels page.
https://warmglass.com/enamels/
https://warmglass.com/enamels/
Re: A-14?
Read all about it:
https://www.aaeglass.com/media/download ... _guide.pdf
• A-14 was by far the best mixing medium I found to use with these enamels. This can be found
here at AAE Glass https://www.aaeglass.com/a-14-enamel-pa ... nprinting-
enamel-2oz-bottle.html The enamel particles mixed well with this medium and the material
was very smooth and uniform. Easy application as well. Great for screen printing and hand
Good luck!!
EDIT: Dunno why that last part : A-14 was by far....... isn't shown as a quote, which it should be, otherwise I've slipped into automatic writing territory. Creepy!
https://www.aaeglass.com/media/download ... _guide.pdf
• A-14 was by far the best mixing medium I found to use with these enamels. This can be found
here at AAE Glass https://www.aaeglass.com/a-14-enamel-pa ... nprinting-
enamel-2oz-bottle.html The enamel particles mixed well with this medium and the material
was very smooth and uniform. Easy application as well. Great for screen printing and hand
Good luck!!
EDIT: Dunno why that last part : A-14 was by far....... isn't shown as a quote, which it should be, otherwise I've slipped into automatic writing territory. Creepy!