HI,
Does anyone have any experience stacking shelves in the Evenheat "coffin"? I need to fire polish 15 pounds of 10 mm square thin bullseye pieces.
If I put a layer directly on the bottom (using fiber paper) and then a layer of kiln shelves above that, I figure I can get 4 cut up sheets in at a time. Or nearly.
Am I going to have a real uneven batch ie top layer will be more exposed to heat than bottom and thus "fired more" than the pieces on the bottom?
Thanks,
JC