Page 1 of 1

Do you have fusing and annealing temps for 104 coe

Posted: Sat Sep 08, 2012 1:23 pm
by lorwolff
I have lost my notes for firing Effetre soft glass.
I would like to try something with rods and murrini, but do not remember the full fuse temp, or best annealing tempurature.

Has anyone here done fusing with this mainly bead making glass?

Re: Do you have fusing and annealing temps for 104 coe

Posted: Sun Sep 09, 2012 6:26 pm
by Stephen Richard
Here is a table from Kirwan that might be useful
http://glasstips.blogspot.co.uk/2010/07 ... fetre.html