Page 1 of 1
hire fire glue?
Posted: Wed Jan 22, 2014 9:32 pm
by Babette (Shawn)
Is there any glue that will hold glass together at slumping temperatures? I slump at about 1100F.
Re: hire fire glue?
Posted: Wed Jan 22, 2014 10:28 pm
by Terry Curtis
what are you trying to do? Are you trying to avoid an extra firing instead of first doing a tack fuse and then slumping?
Re: hire fire glue?
Posted: Wed Jan 22, 2014 11:00 pm
by charlie
i doubt it. most glues are organic, and organics can't usually last that high. there may be some hi-temp epoxies; for instance, you can use some epoxies on car headers, which probably reach 800-900F or so.