reading BE reactive chart
Posted: Wed Dec 17, 2014 12:35 am
by vblue
I was looking at Bullseye reactive glass chart. I'm not sure I'm reading it correctly.
Can you get reactions from any of the transparent glasses? Most of those listed say "opal".
Thanks,
Vernelle
Re: reading BE reactive chart
Posted: Wed Dec 17, 2014 4:31 pm
by jim burchett
The chart is pretty clear..you get reactions from the glasses listed..if it says opal then opal is where the reaction is
Re: reading BE reactive chart
Posted: Wed Dec 17, 2014 5:19 pm
by Morganica
Make sure you're looking at the latest version:
http://www.bullseyeglass.com/images/sto ... _glass.pdf
The older versions used to list the transparent and opal glasses separately. The new chart mixes them up.
Opal glasses will have a 0 in the 4th from last position in the product number, as in "000208." Transparent glasses will have a 1 in that position, as in "001818."