Page 1 of 1
BE 1411, anyone knows????
Posted: Thu Apr 06, 2017 11:25 am
by Havi
Hello good friends,
Lately I bought some glass sheets, from someone who closed his workshop, .
Among them BUllseye 1411 - which looks reddish.
It does not appear on the online catalog, and/ or the written catalog of BE. But it HAS a BE label on it!
Can anyone tell me what it is?
Many thanks in advance,
Havi
Re: BE 1411, anyone knows????
Posted: Thu Apr 06, 2017 12:09 pm
by Brad Walker
Deep Plum Transparent:
http://shop.bullseyeglass.com/catalog/p ... 8/id/1411/
Not sure if it's the same as 1105, which has the same name.
You might want to ask Bullseye for clarification.
Re: BE 1411, anyone knows????
Posted: Thu Apr 06, 2017 3:54 pm
by Havi
Many thanks, Brad!
Havi
Re: BE 1411, anyone knows????
Posted: Fri Apr 07, 2017 10:27 am
by The Hobbyist
It was my mother's favorite color. It went out of production years ago but I made it my quest to acquire a bunch. She's passed and I still have a lot left, mostly thin and a couple halfs with irid.
It's a luscious deep pink/purple/plum. It is very close to Cranberry Pink 1311. It too was a striker and the cold sheet can vary considerably before firing. I've made a couple awesome square dishes using homemade 1411 frit and 1821 Erbium Pink frit.
Jim "The Hobbyist"
Re: BE 1411, anyone knows????
Posted: Fri Apr 07, 2017 11:39 am
by Havi
Many thanks!
The glass I bought is 1.5 millimeter, few sheets of it.
We'll see what happens with it.
There is another 'something' red that I bought which is not on the catalog - but this one I do not recall the number.
I'll post a question later.
Thanks again, you are the best!
Havi
Re: BE 1411, anyone knows????
Posted: Fri Apr 07, 2017 12:12 pm
by DonMcClennen
I still have some 1311 and 1411 on my shelf... both were very $$ glass.. beautiful when fired! Don't waste it!!
Re: BE 1411, anyone knows????
Posted: Fri Apr 07, 2017 1:04 pm
by Havi
OK,
Thanks Don
Havi