When a color doesn't strike
Posted: Thu Apr 12, 2018 12:20 pm
Can a color that didn't strike on the 1st time through the kiln (violet striker, #1234, came out a muddy transparent blue depending on the light) go through the kiln again to reach it's intended color or is it now scrap? I didn't hold it for 2 hours at 1225.