Has anyone tried doing a pot melt onto fiber paper or Thin Fire?
Thanks
Michael
Posted: Tue Feb 24, 2004 1:00 pm
by charlie
yes. don't. it will pull up fibers or dust into the glass, cause ugliness at the best, and incompatibilities and cracking at the worst.
i use a piece of glass for the melt to land on, and very fine layer of baby talc under that to allow the glass to slide without sticking.
Posted: Thu Feb 26, 2004 12:33 am
by Tyler Frisby
Any problems trying a Pot melt into a plaster/silica mold ? Ive thought It would be really swank to try