Page 1 of 1
home made glass globs.
Posted: Sun Apr 06, 2003 4:50 pm
by linda s
Thankyou for so much info on the previous thread. So if I make my own ... Hows this sound? Strip cut 1/2" squares, knock off the corners slightly with the grinder, stack it 4 layers high and fuse. We should petition bullseye to make globs. Thanks
![Razz :P](./images/smilies/icon_razz.gif)
Posted: Sun Apr 06, 2003 5:11 pm
by cindyj
I imagine there a zillion techniques for making globs. Mine are generally only 2-3 layers thick. I tend to go slightly smaller than 1/2 inch and I don't bother to knock of any corners. Just stack (a little glue) an dfire away. I take mine up higher than any other firings to make them round off. I do them in my hot box vs big kiln and they go up to around 1650.
Good luck.